    Default Polished Nano Solid

    Does anyone have experience with a polished Nano. Trying to tame the over under my lane conditions give me every week.

  2. #2
    Step into my office


    The Mayor's Avatar
    Join Date
    Nov 2009
    Location
    Orange City, FL
    Posts
    1,046
    Chats: 42

    Default

    Are you talking about the NANO Pearl? Or do you have a NANO Solid that is polished?

    If you've got the pearl, you can take the finish down to say 4000 abralon with no polish or even 1000 with polish and that should help with the over/under.
    My new CD, 'What I'm Made Of' is available now at www.dustinseymour.com, iTunes, Amazon and more!

    I'm a bowler and a musician. I have a strong love for both. www.facebook.com/dustinseymourmusic

    I am a proud member of Bowlingboards.com bowling Forums.

  3. #3

    Default

    I have the Nano Solid at OOB. I play on a THS that plays more like a sport shot due to heavy oil at the end of the pattern. I know on heavy oil that gives a over/under type shot that weaker is better. I was wondering if any has polished the nano and how it worked for them.

    I'm thinking about 1500 + polish or 500-1000/polish